Common Name(s): White Ash, American White Ash Scientific Name: Fraxinus americana Distribution: Eastern North America Tree Size: 65-100 ft (20-30 m) tall, 2-5 ft (.6-1.5 m) trunk diameter Average Dried Weight: 42 lbs/ft3 (675 kg/m3) Specific Gravity (Basic, 12% MC): .55, .67 Janka Hardness: 1,320 lbf (5,870 N) Modulus of Rupture: 15,000 lbf/in2 (103.5 MPa) … Continue reading White Ash