> Hardwoods > Fabaceae > Acacia > melanoxylon Common Name(s): Australian blackwood, Scientific Name: Distribution: Native to Tasmania and eastern Australia; also introduced to Africa, South America, and southern Asia Tree Size: 65-100 ft (20-30 m) tall, 2-3 ft (.6-1 m) trunk diameter Average Dried Weight: lbs/ft3 ( kg/m3) Specific Gravity (Basic, 12% MC): , … Continue reading Australian Blackwood